Abstract
Fe-doped ZnO nanowires (FZO-NWs) in microfibrous regime were successfully synthesized via a facile dip −coating method. The post deposited films were characterized by X-Ray diffraction (XRD) analysis, scanning electron microscope (SEM), Atomic Force microscope (AFM) and UV–vis spectrophotometer. Besides this, their photocatalytic activities were investigated through orange II dye (O-II) degradation. XRD analysis showed that FZO-NWs have been attached to the bulk wurtzite ZnO and ZnFe2O4 crystalline phases. SEM images clearly show the perfect hexagonal geometry of NWs in micro fibrous regime, with a width size ranged from 0.75 to 3.93μm. The RMS surface roughness are varied in a wide range (7.57–4.,9nm). The UV–vis absorption threshold is shifted from 3.25eV to 3.15eV. The recorded data demonstrated that FZO possessed significant photocatalytic activity. Especially, 5% Fe-ZnO-NWs gave the best degree of decolarization 42% then pure ZnO 25% within 350min.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.