Abstract

The development of an ultrafine grained carbon steel during repetitive shear deformation of side extrusion and the properties after heat treatment were investigated. Side extrusions were carried out at room temperature and the used material was 0.50% carbon steel. The repetitive side extrusions with a constant lateral pressure were carried out up to 3 passes without rotation. The specimens of these steels after 3 passes were annealed at a constant temperature of 600°C changing the treatment time. After side extrusion and heat treatment, the fatigue property was better than that of the as-received material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.