Abstract

Abstract The surfaces of Ti17 alloy were strengthened by an electric spark treatment (EST), then an ultrasonic surface treatment was used in order to improve the fatigue life. The surface morphology was observed by SEM. The surface residual stress was analyzed by a X-ray diffractometer. Tension-tension fatigue tests were carried out in a HT-100 fatigue testing machine at 350 °C. The results show that the surface roughness and the residual stress are reduced for the specimens after the ultrasonic treatment. The fatigue life of the specimens strengthened by ultrasonic treatments is about twice that of the specimens treated by EST only. The fatigue life of the specimen strengthened by YG8 electrode EST combination with ultrasonic treatment is the longest.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.