This paper describes the fatigue behaviour of newly developed all-polypropylene (all-PP) tapes and composites, with reference to the composite processing conditions, testing temperature and making a comparison with commercial alternatives. All-PP tapes are highly oriented and their failure behaviour follows that of other highly oriented polymers. All-PP woven composites fail ultimately due to PP tape failure. However, this failure mode is accompanied by delamination of fabrics in the woven structure. Consolidation pressure plays a decisive role in controlling the interlaminar properties and hence the delamination resistance and furthermore the fatigue limit of the composite. Comparison of all-PP woven composites with commercial alternatives based on glass and natural fibres reveals the excellent relative performance of all-PP composites under fatigue loads. Fatigue properties of all-PP composites are however sensitive to the testing temperature, and elevated temperatures can lead to a rapid reduction of the fatigue resistance of these all-polymer systems.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call