Classical stress-life (S-N) curves were developed for Association of American Railroads (AAR) Class A wheel steel with specimens removed from the rim area of an as-forged railcar wheel. The specimen geometry was a standard hourglass fatigue test specimen with a low stress concentration (Kt) of 1.05. Fatigue testing was performed at stress ratios of −1.0, 0.05, 0.5 and 0.7. Testing was performed at ambient, 500° F and 1000° F using high current resistance or convection methods. Endurance limit data was obtained for all R-ratios, although for the 1000° F condition there did not appear to be a clear endurance limit transition. These endurance limit data were used to estimate the Sines parameters, A and α.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.