Abstract

Abstract Large and hard inclusions often deteriorate the service performance and reduce the fatigue lifetime of drill rods. In this paper, the main reasons of the rupture of drill rods were analyzed by the examination of their fracture and it is found that the large inclusions were the main reason of breakage of rod drill. The inclusions were high of Ca content or Al2O3 rich. Smaller and better deformability inclusions were obtained by the optimization of refining slag, calcium treatment process and the flow control devices of tundish. Results of industrial experiment after optimization show that total oxygen content of drill rods decreased by more than 50%, macro-inclusions weight fraction decreased from about 4 mg/10 kg to about 0.3 mg/10 kg and the micro-inclusions average size decreased from 6 to 3.6 μm. The average using times of drill rods after optimization were increased by about 60%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.