This paper presents test results of AA2519/TI6AL4V composite laminate structure and mechanical properties. The composite laminate was merged by explosive welding using a transition AA1050 alloy layer. The tested composite after formation was annealed, quenched in water and then aged to strengthen it. The heat treatment process was carried out in order to improve the physical and strength properties of the laminate. Weld endurance properties were determined through fatigue testing performed in constant total deformation amplitude (εac) conditions.The paper also describes the influence of test conditions on hysteresis loop shape, process of cyclic material strengthening and weakening, and fatigue life. Low cycle test results were approximated using a straight line with the following formula: σa = K'(εap)n which enables the K'fatigue strength coefficient, and the n' cyclic strengthening index to be determined. Test results also include fatigue fracture surface analysis. Distinctive fatigue fissure characteristics were investigated through studying fatigue fracture surface microstructure using a scanning electron microscope.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.