Abstract

An experimental approach using a modified four ball machine has been used to investigate the rolling contact fatigue (RCF) performance and failure modes of WC-12Co coated rolling elements deposited by the high velocity oxyfuel (HVOF) process. The rolling elements were in the form of12·7 mm diameter M50 bearing steel rolling element balls. The RCF tests were conducted under various tribological conditions of contact loading in conventional steel ball bearing and hybrid ceramic bearing configurations. Results indicate that the rolling elements failed at contactloads above 2·4 GPa and that the failure mode was coated delamination at the coating/substrate interface. Moreover, an appreciable amount of surface wear was observed on the surface of the rolling elements after the RCF tests. The test results and failure modes are discussed in thecontext of the coating/substrate microhardness results, elastohydrodynamic lubrication (EHL) regimes, surface observation of the failed areas using scanning electron microscopy (SEM), slip analysis, frictional torque measurements, and stress contours developed by finite element modelling ofthe coated rolling element ball. Solutions to resist interfacial delamination are also discussed

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.