Abstract

The growth of nano-sized macropores at high speed is studied in this work. Nice macropores with diameters of 60–100 nm and aspect ratio up to 2500 were formed by anodic etching on highly-doped n-type silicon without illumination. The HF-containing electrolytes were modulated with strong oxidizer, H 2O 2, which was also attempted by a few other researchers, but did not lead to the expected macropore formation. Our findings reveal that the pore morphology and etching speed are on dependence of HF concentration and the applied current density. The parameter window of macropore formation, corresponding to the HF concentration ranging from 33% to 67% (by volume) in our experiment, is rather large. In addition, the growth speed can be driven up to 1800 μm/h, while the pores are straight, cylindrical and rather smooth. The current-burst-model is applied to interpret the mechanism of such nano-sized macropore formation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.