We report the development of over 100 μm/h growth rate process on 4-inch diameter wafers using chlorinated growth. The optimized growth process has shown extremely smooth epilayers completely free of surface step-bunching with very low surface defect density, high uniformity in thickness and doping and high run to run reproducibility in growth rate, controlled doping and defect density.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.