Abstract

We report the development of over 100 μm/h growth rate process on 4-inch diameter wafers using chlorinated growth. The optimized growth process has shown extremely smooth epilayers completely free of surface step-bunching with very low surface defect density, high uniformity in thickness and doping and high run to run reproducibility in growth rate, controlled doping and defect density.