Abstract
The composite of paraffin with reduced graphene oxide (paraffin/rGO) was obtained at 70 °C by the mechanical mixing of the components followed by ultrasonic dispersion. The introduction of only 0.3 wt.% rGO stained the paraffin black. It has been shown that thermal batteries made from 160 grams of pure paraffin and 160 grams of the composite are equally slow at charging when placed in boiling water. However, two minutes of microwave heating increases the temperature of the pure paraffin battery to only 32 °C, while the temperature of the paraffin/rGO composite battery rises to 74 °C, which is above the paraffin solid–liquid phase transition temperature.
Published Version (Free)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.