Abstract

Objectives: This study was examined thesurface microhardness of three kind of bulk fillcomposites Surefil SDR flow, Tetric, EvoCeram,X-tra base)Materials and Methods: Ten specimens of2mm, 4mm thickness and 4mm diameter of eachbulk fill composite were polymerized using ahalogen light and a blue light-emitted diode.Microhardness evaluation was performed at the topand bottom surfaces for each specimen using aVickers microhardness tester.Results: All of the materials were cured withthe light sources and the values obtained for thebottom surfaces were found to be lower than thevalues of top surfaces. Highest microhardness level(40.02±4.06)among all composite materialsbelonged to Xtra base composite group, whereaslowest microhardness level (5.80±0.83) was ofSDR composite specimens.Conclusions: Hardness ratio range was between0.19±0.3 and 0.72±0.06. Hardness ratio value wasfound to be lower than 0.80 for all compositegroups.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.