Abstract

In order to clarify the Pb 2+ contribution to the magneto-optical and magnetic properties in garnets (Pb 2+, Th 4+)-substituted YIG were grown by an LPE method onto gadolinium-gallium garnet (GGG) substrates and the Faraday rotation (FR) in the visible wavelength region and the Curie temperature T C were measured. A large negative FR was observed and the FR per Pb 2+ ion at 633 nm was found to be about 80% of that per Bi 3+ ion. T C increases with the increase of Pb 2+ in the films and Pb 2+ contribution to T C was found to be about 60% of Bi 3+ one.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.