Abstract
The steady-state stress distributions in single- and multi-material notched and waisted specimens were investigated for practical creep test specimens using material properties obtained for materials from a service-aged CrMoV pipe weldment. The tri-axial stress conditions existing in notched and waisted specimens machined from welded pipes were identified. By using a steady-state effective failure stress, it has been shown that an approximate method, based on steady-state stress, for the prediction of rupture life and failure position can produce reasonably accurate results. The applicability of the approximate method was confirmed by comparing the results obtained using it with those obtained from corresponding creep continuum damage modelling. These results indicate that use of steady-state stress analysis, as an approximate technique, may be useful for assessing creep failure behaviour, for determining the effect of specimen size and for generating material properties for welded components.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.