Abstract
Based on a system of macro & micro fracture appearance observation, energy spectrum analysis, metallurgical structure inspection and hardness test, the fracture mechanism and cause of specimen of 16Mn steel were obtained. The results showed that the large load was the main reason for the 16Mn steel specimen fracture, the fracture surfaces were different dimensional equiaxed dimples and some spherical particles which contain higher Mn, Si and O. The spherical particles may be an oxide which may be caused by the manufacturing process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.