Abstract

In this study, failure analysis of the 1657CCGA package with 95.5wt%Sn3.9wt%Ag0.6wt%Cu and 63wt%Sn37wt%Pb solder pastes on lead-free PCBs with the Entek OSP (organic solderability preservative) surface finish is investigated. Emphasis is placed on determining the failure locations and failure modes of the solder joints of the 1657CCGA assemblies after they have been through 7,000 cycles of temperature cycling.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.