Abstract

Polyacrylonitrile/poly(acrylic acid) (PAN/PAA with weight radios of 3/7, 4/6, 5/5, 6/4, 7/3 and 10/0) nanofibers (NFs) were prepared as filter medium by electrospinning. The tensile strength of blended nanofibrous mats increased as increasing PAA content, from 3.8 to 6.6 MPa, higher than pristine PAN. The mesoporous effect of nanofibrous mats was also investigated from the nitrogen physisorption isotherms, average pore size in the range of 17–44 nm. Air filtration efficiency and pressure drop of nanofibrous mats were evaluated. PAN/PAA (6/4) NFs showed high filtration efficiency (99.994 %) with lowest pressure drop (160 Pa) for 300–500 nm sodium chloride aerosol particles at a 5.3 cm/s airflow velocity, which suggested this material was appropriate as a promising candidate for high performance filters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.