We present a facile access route to hydroxy-functional narrow disperse microspheres of well-defined grafting density (GD). Ethylene oxide has been grafted from highly crosslinked poly(divinyl benzene) microspheres by anionic ring-opening polymerization using sec-butyllithium as activator together with the phosphazene base t-BuP(4) . Initially, core microspheres have been prepared by precipitation polymerization utilizing divinyl benzene (DVB, 80 wt.-%). The grafting of poly(ethylene oxide) (PEO) from the surface resulted in the formation of functional core-shell microspheres with hydroxy-terminal end groups. The number average particle diameter of the grafted microspheres was 3.6 µm and the particle weight increased by 5.7%. The microspheres were characterized by SEM, FT-IR spectroscopy, elemental analysis, and fluorescence microscopy. The surface GD (determined via two methods) was 1.65 ± 0.06 and 2.09 ± 0.08 chains · nm(-2) , respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.