Abstract

Composites of TiC and TiB2 (TiC-TiB2) were prepared by self-propagating high-temperature synthesis (SHS), using compacted reactant different combinations of Ti, C, and B powders. It is very difficult to densify these materials using conventional sintering techniques. It was found that the chemical reaction between the starting Titanium, boron and carbon particles could be completed at 1200°C producing a pure TiB2+TiC ceramic composite. Various carbon content causes the microstructure of the final products was different.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.