Abstract

Mesoporous zirconias were prepared by precipitation method using rosin-based quaternary ammonium salt as a directing agent. The samples were characterized by means of XRD, FT-IR and N2-adsorption and desorption measurements. The phase of precursors was amorphous, and well crystallized tetragonal zirconias were obtained after the calcination at 450 °C. The synthesized mesoporous zirconias possessed high surface areas ranging from 183.56 to 203.87 m2g-1and big pore diameters varying from 6.27 to 7.58 nm. The content of the rosin-based quaternary ammonium salt had significant influence on the textural properties of the mesoporous zirconias. Surface areas, pore volumes and pore diameters of the mesoporous zirconias decreased when increasing the surfactant dosage.