Abstract
The interaction of magnesium carbonate with polyphenylsiloxane under the conditions of mechanochemical activation with subsequent heating has been investigated. Based on the TGA and DTA data, it has been shown that, upon heating up to 420°C, the reaction proceeded completely with the release of carbon dioxide. The polymer was dissolved in DMFA and purified by repeated precipitation with water. The polymer yield was 64%. The residue insoluble in organic solvents has been obtained by evaporation of an aqueous solution. The composition and structure of the synthesis products have been analyzed by means of element analysis, IR spectroscopy, and diffractometry. It has been demonstrated that the fraction soluble in DMFA had a silicon-to-magnesium ratio equal to 4.2, while the fraction isolated from water had this ratio equal to 1.0. The IR and XRD data enabled one to conclude that, regardless of the different compositions, the structures of all fractions were similar and corresponded to mesomorphic layered polymers produced by the ion exchange method.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.