Abstract

Low or zero thermal expansion porous ceramics are required for several applications. In this work near zero thermal expansion porous ceramics were fabricated by using SiC and ZrW2O8 as positive and negative thermal expansion materials, respectively, bonded by soda lime glass. The mixture of SiC, ZrW2O8 and soda lime glass was sintered by Pulsed Electric Current Sintering (PECS, or sometimes called Spark Plasma Sintering, SPS) at 700 °C. Sintered samples with ZrW2O8 particle size smaller than 25 μm have high thermal expansion coefficient, because ZrW2O8 has the reaction with soda lime glass to form Na2ZrW3O12 during sintering process. The reaction between soda lime glass and ZrW2O8 is reduced by increasing particle size of ZrW2O8. Sintered sample with ZrW2O8 particle size 45-90 μm shows near zero thermal expansion.