Abstract
Abstract A novel anode electrode consisting of Pt NPs on layered porous TiO2/CFP (Pt/LP-TiO2/CFP) was fabricated by an innovative approach, which can be directly integrated in membrane electrode assembly (MEA) as the catalyst layer without any binder. Firstly, a two-step anodization method was applied to prepare a layered porous TiO2 on the CFP as a hybrid support, and then Pt NPs are deposited onto it by atomic layer deposition (ALD) technology. It effectively prevents Pt nanoparticles from detachment, migration, and aggregation during the catalyst preparation and electrochemical reaction process. The electrocatalytic performance of Pt/LP-TiO2/CFP electrode for methanol oxidation reaction exhibits excellent mass activity (1182.8 mA mgPt−1), enhanced stability, and CO tolerance, which is much better than those of the Pt/HT-TiO2/CFP and the Pt/C/CFP electrode prepared by conventional hydrothermal and spray method, respectively. The reason can be attributed to the unique structure of layered porous TiO2 supports, strong metal−support interactions (SMSI) between ALD Pt NPs and the LP-TiO2/CFP, and more exposed active sites for methanol oxidation. The presented ALD approach is an effective strategy for the homogeneous distribution of precious Pt nanoparticles on a binder-free and porous electrode for the design of advanced catalysts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.