Abstract

La₂O₃-TiO₂-SiO₂ glass, a type that could not obtained so far by the conventional melting method, was prepared successfully using a sol-gel process. Glass derived with the sol-gel process has compositions of 5La₂O₃-5TiO₂-90SiO₂, 5La₂O₃-10TiO₂-85SiO₂, and 5La₂O₃-20TiO₂-75SiO₂. The UV-visible absorption edge of all glass compositions was below 400 ㎚. The measured density is in the range of 2.55-2.89, and was nearly identical to the calculated density and the refractive index of the glasses derived from the sol-gel ranges from 1.545 to 1.645. The molar additive coefficient of TiO₂ measured in this ternary system is lower than the calculated value, while the value of La₂O₃ is higher.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.