Abstract

A simple method to indium tin alloy and oxide nanowires were achieved by using the extrusion molding process in the air. Eutectic indium tin bulk were firstly injected into AAO templates. After dissolving AAO, the indium tin nanowires were collected in ethanol. Furthermore, in order to have oxide nanowires, alloy nanowires were directly oxidized by heat treatment in the air below its melting point for 24 hours. Finally, crystalline indium-tin oxide and indium oxide nanowires with diameters 90-110 nm and lengths 2-20 μm were obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.