Abstract
AbstractConformal parallel arrays of Al‐doped TiO2 nanotubes were fabricated by atomic layer deposition. TiO2/Al2O3 bilayered shells were grown on a polycarbonate template by various cyclic sequences of TiO2 and Al2O3. The doping level of Al could be tuned by the fraction of cycle number of Al2O3. From the depth profiles measured by second ion mass spectrometry, Al is uniformly distributed across the thickness, which is also supported by the analyses of X‐ray diffraction, X‐ray photoelectron spectroscopy, and Raman spectroscopy. A uniform bulk solubility of ~7 at.% and the surface concentration of ~18 at.% were observed with the cycle ratio of Al2O3: TiO2 at 0.04.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.