The FePt films were fabricated by using RF sputtering for magnetic recording media. The efforts have been done to reduce the grain size, to decrease the ordering temperature, and to control the crystalline orientation. It was found that the proper amount of alumina led to decrease the grain size and weak the interparticle exchange coupling. 15% N 2 partial pressure can reduce the transform temperature from fcc to fct phase. In order to control the texture in the FePt films, two kinds of methods were used. On the one hand, the addition of W in Cr underlayer and the usage of Mo and Pt as intermediate layer caused the texture of FePt films changed from (200) to (001). On the other hand, the (Pt/Fe) n multilayers were fabricated to produce the FePt (001) orientation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.