To remove the arsenic from gold concentrate using a thermal decomposition method, a test was conducted while changing the reaction time at 700°C. Additionally, the volatile arsenic from the gold concentrate was recovered using a bag-filter. The arsenic content in the concentrate was rapidly reduced from 12.62wt.% to 1.40wt.% after 1-hour burning and to below 1wt.% after 2 hours, indicating approximate 95% removal rate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.