Abstract

Limited CFETR-scale experience of engineering preparation techniques of tritium permeation barrier (TPB) exists up to date. Aimed at processing some real components that are usually tubular components sealed in one end, in the tritium cycling systems of China Fusion Engineering Test Reactor (CFETR), an Al2O3/FeAl coatings as TPB was prepared on tubular components of 321 type stainless steel components with a length of 400 mm and an external diameter of 150 mm, by Al-electroplating followed by heat treating and selective oxidation. The ability to construct TPB coated components on quasi-CFETR scale was demonstrated, with fabricating a TPB of Al2O3/FeAl coating with a double-layered structure, consisted of an outer γ-Al2O3 layer with a thickness of 0.3 µm and an inner (Fe,Cr,Ni)Al/(Fe,Cr,Ni)3Al layer of 40 µm in thickness. The tritium permeation reduction factors of the Al2O3/FeAl TPB on component were 229 and 96 at 500 and 600 °C respectively. Finally, signatures and gaps of TPB mass process on CFETR-scale were discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.