Abstract

In this paper we report on the preparation and laser performance of transparent 3at.% Yb:Sc2O3 ceramics by reactive sintering of commercially available powders under vacuum followed by hot isostatic pressing (HIP). Combinations of different vacuum sintering temperatures (1650 °C and 1750 °C) and different HIP treatments (1700 °C and 1800 °C at 200 MPa) were tested in order to understand how these steps influence the microstructure and thus the optical and lasing properties of the ceramic samples. All the samples showed a good optical quality. The microstructure analysis and the laser tests showed that the vacuum pre-sintering temperature is the key factor determining the quality of the samples and the laser performances. The best values of slope efficiency i.e. ηL = 50 % and output power i.e. Pout = 6.62 W were obtained for the sample pre-sintered under vacuum at 1650 °C and hot isostatically pressed at 1800 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.