Abstract

By conducting the orthogonal design for the best mechanical properties of the matrix parts without introducing air pores in advance, the self-ignition coal gangue: lime: cement: gypsum=54: 23: 20: 3 accompany with 1.3‰ aluminum powder is determined as the optimal mix proportion of the self-ignition coal gangue aerated concrete. Meanwhile, the reasonable Ca/Si ratio of the elements is found to be 0.82. XRD results show that the hydration products of self-ignition coal gangue autoclaved aerated concrete (SCGAAC) are mainly consisted by CSH gel and tobermorite phase, moreover, SEM approved that a higher Ca/Si ratio is conducive to form the tobermorite phase under the autoclaved conditions. The induced pores in SCGAAC are mainly interconnected open cell structure with middle characteristic latitudinal dimension between 0.5 and 2mm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.