Abstract
To form a tungsten disulfide film, a tungsten trioxide film is deposited first and then hydrogen sulfide is injected into the furnace tube to sulfide the tungsten trioxide film in a high-temperature environment. Due to the need to accurately control the thickness of tungsten trioxide, the power of the RF sputtering machine was reduced as much as possible in a stable condition in the experiment and the bias voltage during each process was monitored. In this experiment, a sapphire substrate and a silicon substrate with 200[Formula: see text]nm silicon dioxide are used. Then use optical instruments such as Raman optics, ellipsometers and high-resolution electron transmission microscopes, atomic force microscopes and other instruments for further measurement. The analysis results show that we have successfully made tungsten disulfide films of different thicknesses. Moreover, two-dimensional tungsten disulfide thin film has a response to light, gas and pH and related devices have been successfully fabricated in experiments. Among them, comparing the single-layer film and the double-layer film, the film quality of the double-layer film is better. The quality of the film grown on the sapphire substrate is also better than the quality of the film grown on the silicon dioxide substrate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.