Abstract

Because of the hydrophilic characteristics of native starch foams and the cost of modifying starch, the uses of starch and modified starch foams are hindered. To decrease hydrophilicity and cost of starch foams, native corn starch was blended with starch acetate and extruded. A twin-screw mixing extruder was used to produce the foams. Native starch content, screw speed, and barrel temperature had significant effects on molecular degradation of starches during extrusion. The melting temperature of extruded starch acetate/native starch foam was higher (216 degrees C) than that for starch acetate (193.4 degrees C). Strong peaks in the X-ray diffractograms of extruded starch acetate/native starch foam suggested new crystalline regions were formed. Optimum conditions for high radial expansion ratio, high compressibility, low specific mechanical energy requirement, and low water absorption index were 46.0% native starch content, 163 rpm screw speed, and 148 degrees C barrel temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.