Abstract

• The TBP is an effective extractant to remove Fe 3+ from phosphoric acid containing Cl − . • The Fe 3+ was removed completely by a counter-current three-stages extraction. • Fe 3+ was extracted in the form of HFeCl 4 and 2TBP·HFeCl 4 is the formed complex. • Each HFeCl 4 combines two TBP molecules on the opposite sides. • Fe O{TBP} is formed in the extraction process with a bond energy greater than 165 kJ/mol. Fe 3+ is an impurity of the raw phosphoric acid from wet-process route and the waste phosphoric acid from the etching process of electronic industry. The effects of temperature, the Cl − content and TBP dosage on the extraction performance of synthesized extractants to Fe 3+ in raw phosphoric acid from HCl wet-process route were investigated systematically. The results show that the extractant containing 12.5 vol% TBP and 87.5 vol% kerosene effectively extracted Fe 3+ at 293.15 K from raw phosphoric acid containing 15.8 wt% Cl − . The extraction efficiency of 100% was realized by counter-current three-stage extraction. The extract phase was characterized by FT-IR and UV–vis. The results show that Fe 3+ was extracted by TBP with the form of HFeCl 4 . The interaction between TBP and HFeCl 4 was simulated by DFT (density functional theory). The lowest energy structure, electrostatic potential distribution, energy change, bond level analysis, electron transfer, frontline molecular orbital and other information of the possible complex were simulated systematically. The results of the characterization of the extraction phase and DFT simulation were used to clarify the extraction mechanism and the structure of the complex. The simulation results show that the lone-pair electrons of the P O double bond in TBP has a strong complexation interaction with the empty orbital of HFeCl 4 and a strong bond Fe O{TBP} is formed in the extraction process. The bond length of formed Fe O{TBP} is 2.05A, the LBO bond level of Fe O{TBP} is 0.076 (0.075), the Mayer bond level of Fe O{TBP} is about 0.16, the ρ b values of Fe O{TBP} bond critical points range from 0.252 to 0.271 e − /bohr 3 . A minimum electrostatic potential of −50.59 kcal/mol is existed in TBP at the vicinity of O atom in P O double bond. Two maximum electrostatic potential of 69.43 kcal/mol and 69.92 kcal/mol are distributed symmetrically on the opposite sides of the Fe vicinity of HFeCl 4 . Each HFeCl 4 molecule combines two TBP molecules on the opposite sides, and the binding sites are near the O atom of the P O double bond of TBP and near the Fe atom of HFeCl 4 . The absolute value of the binding energy is greater than 165 kJ/mol. The complexation reaction of TBP and HFeCl 4 occurs through the surface electrostatic potential attraction and molecular orbital complementation forms. The results are helpful to understand the extraction mechanism of TBP to extract Fe 3+ from phosphoric acid.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call