Abstract

Weibull parameters extracted from tests of 75 mm Kevlar bundles by Fourier deconvolution produced average Weibull parameters of ma 22:2 and 10a 0:0284; which indicate that filament interactions concentrated the failures over a smaller range of strain. A bundle with filaments varying from 75 to 76.1 mm in length failed with a load‐displacement energy 14% higher than found with uniform filament length. Weibull parameters of ma 12:3 and 10a 0:0305 indicate that filament interactions were reduced and parameters corresponding to single filament testing were obtained rapidly. q 2000 Published by Elsevier Science Ltd.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.