Abstract

Nickel extraction from Morowali laterite ore has been carried out with nitric acid as the solvent. This study aims to determine the effect of nitric acid concentration, temperature, and stirring time on nickel content in laterite ore originating from Morowali. Morowali laterite seeds were extracted using the leaching method using nitric acid as the solvent with various concentrations of 0.5, 1, and 2, temperatures of 30, 60, and 95, and stirring times of 3, 6, and 12. Taguchi analysis was used in this study to obtain the effect of the three parameters used. The results showed that the optimum conditions were obtained at a concentration of 2 molars nitric acid, a temperature of 95°C, and a stirring time of 12 hours, with a nickel content of 16.469 ppm and a nickel recovery percent of 3.88%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.