Abstract

The exsolution of metal cations from oxides under reducing fuel conditions results in the formation of surface metallic nanoparticles, which can reduce Solid Oxide Fuel Cell anode polarization resistance. However, the loss of the B-site cations shifts the stoichiometry of the perovskite oxide. Depending on the amount exsolved and the initial stoichiometry, the exsolution can presumably shift the oxide away from its single-phase perovskite region. Herein, the direct comparison of initially stoichiometric composition Sr(Ti0.3Fe0.63Ni0.07)O3-δ (STFN0) with initially A-site deficient Sr0.95(Ti0.3Fe0.63Ni0.07)O3-δ (STFN5) is conducted and reported. X-ray diffraction along with scanning and transmission electron microscopy analysis of the oxides, which are both reduced at 850 °C in H2/H2O/Ar, shows a similar size and density of exsolved Fe–Ni alloy nanoparticles, albeit with slightly different alloy compositions. Whereas the oxide phase in reduced STFN5 shows a well-ordered perovskite structure, the greater B-site deficiency in reduced STFN0 results in a highly disordered and strained structure. The electrochemical performance of STFN0 anodes is inferior to that of STFN5 anodes, and even worse than SrTi0.3Fe0.7O3-δ (Ni-free) anodes. It appears that an initial Sr deficiency is important to avoid a too-high B-site deficiency after exsolution, which distorts the perovskite structure and impairs electrochemical processes.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.