Abstract
This research group has been demonstrating the significant advantages of using Nb2O5 coatings for functionalizing titanium, aluminium, and stainless steels. Regarding the biomedical sector and considering Ti-6Al-4V alloy, the reactive sputtering technique improved the cell viability, the osteogenic performance of cells involved in the osseointegration process as well as the ability to delay bacterial proliferation. The characteristics of the Nb2O5 coatings were assessed before by using standard methods, which provide information only a few tens of nanometers depth. Given that the Nb2O5 coating fabricated in this work exhibits a thickness of approximately 300 nm, the GE-XANES technique emerges as the most suitable method for this analysis. Additional information was provided with the aid of nanoindentation load-depth (P-h) curves. GE-XANES results indicated the formation of a homogeneous layer of Nb2O5 coating on the Ti-6Al-4V surfaces. The deposition process improved the surface hardness of the Ti-6Al-4V alloy (4.38 GPa versus 5.62 GPa) considering the 2 mN load.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.