Abstract

Abstract In recent years, tannin degradation has been used to obtain tannin materials with an optimal molecular weight distribution (MWD) for synthesizing tannin-formaldehyde (TF) resin with high performance, but the optimal MWD of tannins is still unknown. The excellent formaldehyde reactivity of tannins is the basis for the synthesis of high-performance TF resin. Based on the formaldehyde reactivity of tannins, bayberry tannins and larch tannins were used to explore the optimal MWD of tannins for TF resin synthesis. Progressive solvent precipitation (PSP) was used to obtain tannin fractions with different MWDs. The formaldehyde reactivity of tannins was determined using the modified Stiansy method combined with the standard curve method (GB/T 17657-2013). The bayberry tannin fraction [weight-average molecular weight (Mw) of acetylated tannin: 4115, mean degree of polymerization (mDP): 6.64] and the larch tannin fraction (Mw of acetylated tannin: 3906, mDP: 5.84) had the best formaldehyde reactivity. Furthermore, significant differences in the formaldehyde reactivity of condensed tannins (CTs) with different MWDs were observed. The obtained results can be used to purposefully degrade tannins to achieve an optimal MWD, which is beneficial for the production of TF adhesives with high performance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.