Abstract

Strategies to achieve p-type behavior in semiconductor oxides are an important current topic of research. Our study showed that sodium-doped zinc oxide thin films are a plausible approach. The insertion of dopant allowed a transition between n-type p-type electrical behavior in specific temperature ranges around 300 K. Annealing procedures under controlled atmospheres, including Ar, N2, and O2, increased the hole density up to a magnitude of 1016 cm−3, although this also reduced the window temperature. The micro-photoluminescence spectra showed an enhancement of defect-related emissions as the dopant content increased. Notably, yellow-green emissions (around 2.38 eV–520 nm) were the most prominent in the as-grown samples. After annealing, a strong redshift of the defect band was observed (around 1.85 eV–670 nm). Our findings showed that p-type ZnO:Na films exhibited emissions associated with RGB primary colors. In a chromaticity diagram, as-grown samples appeared near the white range, annealed films were close to the warm white area, and O2 annealed films trended within the red range.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call