Abstract

Abstract: Thick films of pure Tin oxide (SnO2) and composite 1%, 3%, 5%, 7% and 9 % tungsten oxide (WO3) incorporated into pure Tin oxide (SnO2) were prepared with standard screen printing technique. All samples were prepared on glass substrate and subjected to drying and firing at 5000C at 5 hours in muffle furnace. Thick films of tin oxide (SnO2) and composite 1%, 3%, 5%, 7% and 9 % Tungsten Oxide (WO3) incorporated into pure tin oxide (SnO2) were examined for Scanning Electron Microscopy (S.E.M), Energy Dispersive X-ray Analysis (E.D.A.X), X-ray diffraction (X.R.D), Fourier Transform infra-Red (F.T.I.R) and Ultra-Violet-visible spectroscopy (U.V) to investigate surface morphology, elemental analysis, crystalline Phases of films, vibrational and spectroscopic study respectively. The spectrophotometric parameters such as absorbance and absorption coefficient were also a part of investigation. The UV-visible spectrophotometric study was encountered in terms of absorbance and absorption coefficient along with varying percentage composition.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call