Abstract The powerful tool for defect analysis is an expert system. It is a computer programme based on the knowledge of experts for solving the quality of castings. We present the expert system developed in the VSB-Technical University of Ostrava called ‘ESWOD’. The ESWOD programme consists of three separate modules: identification, diagnosis / causes and prevention / remedy. The identification of casting defects in the actual form of the system is based on their visual aspect.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.