Abstract
Blast furnace gas ash is one of the main solid wastes in iron and steel enterprise. The recovery of zinc from gas ash can result in considerable economic and environmental benefits. The effect of NH3/NH4+, L/S, [NH3]T and leaching time on the zinc leaching rate of blast furnace gas ash by using ammonia leaching process had been investigated in this paper. The results show that L/S and NH3/NH4+ are the main influence factors under the experimental condition. The optimal conditions for leaching process are: NH3/NH4+=2:1, L/S=4:1, [NH3]T =5mol/L, and the leaching time is 3 hours. The zinc leaching rate is 82.84% under the optimized conditions. The lead content in leaching solution is high, so the main task is to improve the removal rate of lead in the purification process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.