The distribution of trap levels in the low density polyethylene (LDPE) was studied by means of photo-stimulated discharge (PSD). And two scanning modes, continuous scanning and step scanning, were discussed. It was pointed out that there may be some problems because of the incomplete detrapping of the trapping charges for the continuous scanning. The principle and the experimental process for the step scanning were presented. It is found that there is a linear relationship between the logarithm of PSD current produced under the irradiation of the monochromatic light and the time, which is in accordance with the theoretical analysis and indicates that the retrapping effect of the carriers can be neglected. The charges are trapped in the levels of 4.36—6.22 eV in LDPE, the main part of which were trapped in the energy levels of 4.78—5.18 eV.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.