Abstract
Uniform experimental design method is applied to the slow strain rate testing of X12Cr13 stainless steel in natural gas environment. The influence of H2S concentration, CO2 concentration, ambient temperature and pressure on stress corrosion susceptibility are investigated. Through the observation of fracture morphology of the specimens, it is found that the fracture morphology of the specimens is stress corrosion fracture, and there are transgranular, intergranular and mixed fracture. In the fracture energy spectrum analysis, there are many oxides of S and C in the fracture composition, and the content of each element varies greatly with the corrosion environment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.