Abstract

Due to the high tensile strength of ultra-high performance concrete (UHPC), the shear stirrups in UHPC beams could potentially be removed. The aim of this study is to assess the shear performance of non-stirrup UHPC beams. Six UHPC beams were tested and compared with three stirrup-reinforced normal concrete (NC) beams, taking into consideration the testing parameters of steel fiber volume content and shear span-to-depth ratio. The findings demonstrated that incorporating steel fibers can efficiently strengthen the ductility, cracking strength, and shear strength of non-stirrup UHPC beams and alter their failure mode. Additionally, the shear span-to-depth ratio had a significant impact on the shear strength of beams, as it was negatively related to it. This study revealed that the French Standard and PCI-2021 formulae were suitable for designing UHPC beams with 2% steel fibers and no stirrups. When applying Xu's formulae for non-stirrup UHPC beams, taking into account a reduction factor was necessary.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.