Three titanium alloy materials TA7, TB6 and TC4 were selected, and three titanium alloys with different phases were placed in liquid nitrogen at -196°C for cryogenic treatment, and the change of the cutting performance of titanium alloy samples before and after cryogenic treatment was studied.Six speed combinations of 30m/min, 40m/min, 50m/min, 60m/min, 70m/min and 80m/min were selected to carry out cutting tests.The cutting experiments show that the cutting performance of TA7, TB6 and TC4 titanium alloys has been significantly improved by cryogenic treatment.At different cutting speeds, the cutting force was compared. After cryogenic treatment of three titanium alloy materials, the cutting force was reduced in machining.After cryotreatment, the cutting performance of TB6 was significantly improved, while that of TA7 was relatively low. Among them, TB6 showed the greatest improvement, followed by TA7 and TC4.The three titanium alloys without cryogenic treatment have a cutting speed of 50m/min at maximum cutting force.The maximum cutting force speed of cryogenic titanium alloy is 40m/min.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call