Abstract

Solid recycled coarse aggregate concrete bricks were produced by QTY4-40 brick machine with strength grades of MU15-MU30. Recycled aggregate replacement rate was up to 100%. Water absorption and moisture content were tested. Two methods were taken to test the drying shrinkage. The impact of recycled aggregate replacement rate and curing period on the drying shrinkage rate, water absorption, moisture content, density was analyzed, and the relationship between them was presented. The results indicate that recycled aggregate can increase the shrinkage of solid concrete brick. The shrinkage of recycled solid concrete bricks' (fully substitute) is larger than ordinary concrete bricks' by 1.6-2 times. Water reducer is helpful to improve the water retention and decrease the shrinkage of brick. One of the test results of shrinkage got by the methods recommended in relevant specification is smaller.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.