Abstract

According to BS7448 fracture toughness test standard, crack tip opening displacement (CTOD) for ASTM A333 Gr.6 low temperature steel which is used in offshore platform were carried out in low temperature (0°C, -29°C). Three point bending tests were conducted on the specimens, the dimension of which is B×2B (B is the thickness) and notch direction is NP. The final value of CTOD was calculated by P-V curves of both the welds and HAZ (heat affected zone). And the experimental results were analyzed and discussed in the paper. The low temperature steel welded joints show good low temperature toughness, the selected welding procedure is applied to construction of pipelines.The CTOD value of HAZ is larger than weld metal and weld is the weakest position in the whole structure. The experiment results provide an important basis for the choice of welding method and welding process parameters, ECA assessment and construction of offshore platform.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.